Natural Fiber-filled Polypropylene with
2% Polybond 3200 Coupling Agent
Flexural Strength
Note: The fill rate for PlastiCell is only 40% vs. 50% for the other fillers. Size of particle: Wood: 40 mesh; Coconut flour: 100 mesh; Almond Shell Flour: 100 mesh; PlastiCell: L/D = 10+ Conclusion: PlastiCell has 11% higher Flexural Strength than wood, even with 25% more wood used for comparison. Flexural Modulus: We can expect the differences to be even greater with Modulus testing. |